The data is the result of hot deformation tests conducted on magnesium alloy AZ31. It includes stress strain data for a range of deformation conditions and different initial microstructures. It also includes data for the developed grain size and the degree of dynamic recrystallisation
The formability of magnesium alloys can be significantly improved by Ca as an alloying addition. Com...
Kinetics of the dynamic, as well as postdynamic recrystallization of the wrought magnesium alloy AZ3...
High-temperature plastic deformation and dynamic recrystallization of AZ31 extruded (EX) and heat tr...
The deformation behaviour of magnesium alloy AZ31 was examined. The work found that dynamic recrysta...
he microstructural evolution is examined during the hot compression of magnesium alloy AZ31 for both...
The hot working behaviour of magnesium AZ (e. g. AZ31; Al: 3%, Zn: 1%) alloys and their associated c...
Compression tests of magnesium alloy Mg-3Al-1Zn (AZ31) at different temperatures and strain rate wer...
The microstructures of magnesium AZ31 are examined following hot compression testing and annealing. ...
High temperature regime, 300-450°C for Mg-Al-Zn alloys, is currently used in primary processing, suc...
The evolution of flow stress and microstructure for wrought magnesium alloy AZ31 was characterised u...
The present work examines the microstructure that evolves during the hot deformation and subsequent ...
This study presents an analysis of the microstructural evolution and flow stress variation with stra...
This study presents an analysis of the microstructural evolution and flow stress variation with stra...
The hot deformation behavior of an AZ81 magnesium alloy was investigated by hot compressive testing ...
The microstructure and texture evolutions of the Mg–2Zn–0.5Mn–0.2Ca–0.3Nd–0.7La alloy were investiga...
The formability of magnesium alloys can be significantly improved by Ca as an alloying addition. Com...
Kinetics of the dynamic, as well as postdynamic recrystallization of the wrought magnesium alloy AZ3...
High-temperature plastic deformation and dynamic recrystallization of AZ31 extruded (EX) and heat tr...
The deformation behaviour of magnesium alloy AZ31 was examined. The work found that dynamic recrysta...
he microstructural evolution is examined during the hot compression of magnesium alloy AZ31 for both...
The hot working behaviour of magnesium AZ (e. g. AZ31; Al: 3%, Zn: 1%) alloys and their associated c...
Compression tests of magnesium alloy Mg-3Al-1Zn (AZ31) at different temperatures and strain rate wer...
The microstructures of magnesium AZ31 are examined following hot compression testing and annealing. ...
High temperature regime, 300-450°C for Mg-Al-Zn alloys, is currently used in primary processing, suc...
The evolution of flow stress and microstructure for wrought magnesium alloy AZ31 was characterised u...
The present work examines the microstructure that evolves during the hot deformation and subsequent ...
This study presents an analysis of the microstructural evolution and flow stress variation with stra...
This study presents an analysis of the microstructural evolution and flow stress variation with stra...
The hot deformation behavior of an AZ81 magnesium alloy was investigated by hot compressive testing ...
The microstructure and texture evolutions of the Mg–2Zn–0.5Mn–0.2Ca–0.3Nd–0.7La alloy were investiga...
The formability of magnesium alloys can be significantly improved by Ca as an alloying addition. Com...
Kinetics of the dynamic, as well as postdynamic recrystallization of the wrought magnesium alloy AZ3...
High-temperature plastic deformation and dynamic recrystallization of AZ31 extruded (EX) and heat tr...