The influence of Laves phase in the microstructure on the creep strength of a modified 9Cr-1Mo tempered ferritic steel, F91, is investigated in this research. Through additional aging heat treatment up to 5000 h, a pronounced increase of Mo-rich Laves phase is found around Cr-rich carbide M23C6, which is pinned on the prior-austenite grain boundaries and martensitic lath boundaries. This secondary precipitation hardening provided by the Laves phase is rapidly offset by its coarsening into large clusters during long-term thermal exposure and under creep conditions, leading to earlier creep rupture than the pristine material. Uniaxial constant-load creep tests are conducted on both aged and non-aged coupons under the same creep conditions. Th...
The evolution of Fe2(W, Mo) Laves phase in a 3%Co modified P911 heat resistant steel was examined du...
A 9%Cr-3%Co steel with high B and low N contents exhibits creep strength breakdown at a temperature ...
E911 creep samples exposed to temperatures of 600˚C, 625˚C and 650˚C at differing stress levels were...
The influence of Laves phase in the microstructure on the creep strength of a modified 9Cr-1Mo tempe...
The influence of Laves phase (type Fe 2W) formation and growth kinetics on the creep strength at 650...
This paper reports on the formation of an Mo-rich Laves phase during high-temperature exposure and c...
The coarsening of Laves phase in a Re-containing 10% Cr-3% Co-3% W steel during both creep and agein...
Five Co-modified P92-type steels with different contents of Cr,W, Mo, B, N, and Re have been examine...
Long term precipitation and coarsening of Laves-phase in tungsten strengthened 9% Cr steel under the...
The aim of this work was to design 17 wt%Cr Laves phase strengthened HiperFer (Highperfomrance Ferri...
The aim of this work was to design 17 wt%Cr Laves phase strengthened HiperFer ($\textbf{Hi}$gh $\tex...
We report two typical morphologies (elongated- and blocky-shaped) of the Laves phase in tempered mar...
The fine-grained heat-affected zone (FGHAZ) specimens for P92 steel weld were produced by welding th...
The creep behavior of a 3%Co modified P92-type steel with high content of boron and low content of n...
The effect of long-term creep at 600°C under 137 MPa on the microstructure of a P92- type steel was ...
The evolution of Fe2(W, Mo) Laves phase in a 3%Co modified P911 heat resistant steel was examined du...
A 9%Cr-3%Co steel with high B and low N contents exhibits creep strength breakdown at a temperature ...
E911 creep samples exposed to temperatures of 600˚C, 625˚C and 650˚C at differing stress levels were...
The influence of Laves phase in the microstructure on the creep strength of a modified 9Cr-1Mo tempe...
The influence of Laves phase (type Fe 2W) formation and growth kinetics on the creep strength at 650...
This paper reports on the formation of an Mo-rich Laves phase during high-temperature exposure and c...
The coarsening of Laves phase in a Re-containing 10% Cr-3% Co-3% W steel during both creep and agein...
Five Co-modified P92-type steels with different contents of Cr,W, Mo, B, N, and Re have been examine...
Long term precipitation and coarsening of Laves-phase in tungsten strengthened 9% Cr steel under the...
The aim of this work was to design 17 wt%Cr Laves phase strengthened HiperFer (Highperfomrance Ferri...
The aim of this work was to design 17 wt%Cr Laves phase strengthened HiperFer ($\textbf{Hi}$gh $\tex...
We report two typical morphologies (elongated- and blocky-shaped) of the Laves phase in tempered mar...
The fine-grained heat-affected zone (FGHAZ) specimens for P92 steel weld were produced by welding th...
The creep behavior of a 3%Co modified P92-type steel with high content of boron and low content of n...
The effect of long-term creep at 600°C under 137 MPa on the microstructure of a P92- type steel was ...
The evolution of Fe2(W, Mo) Laves phase in a 3%Co modified P911 heat resistant steel was examined du...
A 9%Cr-3%Co steel with high B and low N contents exhibits creep strength breakdown at a temperature ...
E911 creep samples exposed to temperatures of 600˚C, 625˚C and 650˚C at differing stress levels were...