International audienceIn the characteristic gamma/gamma' microstructure of single crystal superalloys, misfit stresses occur due to a significant lattice mismatch of those two phases. The magnitude of this lattice mismatch depends on the chemical composition of both phases as well as on temperature. Furthermore, the lattice mismatch of gamma and gamma' phases can be either positive or negative in sign. The internal stresses caused by such lattice mismatch play a decisive role for the micromechanical processes that lead to the observed macroscopic athermal deformation behavior of these high-temperature alloys. Three-dimensional discrete dislocation dynamics (DDD) simulations are applied to investigate dislocation glide in gamma matrix channe...
International audienceThe initial stages of creep in nickel base superalloy deserve a special attent...
International audienceThe high-temperature creep behavior of a rafted [001] oriented AM1 Ni-based si...
Single crystal Ni-based superalloy, with excellent mechanical properties in high temperature, always...
International audienceThree-dimensional discrete dislocation dynamics (DDD) simulations in combinati...
Abstract. When deforming bulk material, micromechanisms involving moving defects result in mechanica...
International audienceThe high temperature effective (constrained) gamma/gamma' lattice mismatch of ...
Background: Nickel-based superalloys are usually exposed to high static or cyclic loads in non-ambie...
The high temperature effective (constrained) $\gamma/\gamma′$ lattice mismatch of a Ni-based single ...
The structural evolution of misfit dislocation networks at γ/γ′ phase interfaces in Ni-based single ...
A formalism is proposed for the evaluation of phase specific strains and stresses in amp; 947; har...
International audienceComplex thermomechanical loadings at high temperature (T >= 950 degrees C) on ...
In this work, the evolution of the dislocations microstructure in single crystal two-phase superallo...
The dislocation-based modeling of the high-temperature creep of two-phased single-crystal superalloy...
The high-temperature creep behavior of a rafted [001] oriented AM1 Ni-based single crystal superallo...
Einkristalline Superlegierungen werden aufgrund ihrer exzellenten Hochtemperaturbeständigkeit für Tu...
International audienceThe initial stages of creep in nickel base superalloy deserve a special attent...
International audienceThe high-temperature creep behavior of a rafted [001] oriented AM1 Ni-based si...
Single crystal Ni-based superalloy, with excellent mechanical properties in high temperature, always...
International audienceThree-dimensional discrete dislocation dynamics (DDD) simulations in combinati...
Abstract. When deforming bulk material, micromechanisms involving moving defects result in mechanica...
International audienceThe high temperature effective (constrained) gamma/gamma' lattice mismatch of ...
Background: Nickel-based superalloys are usually exposed to high static or cyclic loads in non-ambie...
The high temperature effective (constrained) $\gamma/\gamma′$ lattice mismatch of a Ni-based single ...
The structural evolution of misfit dislocation networks at γ/γ′ phase interfaces in Ni-based single ...
A formalism is proposed for the evaluation of phase specific strains and stresses in amp; 947; har...
International audienceComplex thermomechanical loadings at high temperature (T >= 950 degrees C) on ...
In this work, the evolution of the dislocations microstructure in single crystal two-phase superallo...
The dislocation-based modeling of the high-temperature creep of two-phased single-crystal superalloy...
The high-temperature creep behavior of a rafted [001] oriented AM1 Ni-based single crystal superallo...
Einkristalline Superlegierungen werden aufgrund ihrer exzellenten Hochtemperaturbeständigkeit für Tu...
International audienceThe initial stages of creep in nickel base superalloy deserve a special attent...
International audienceThe high-temperature creep behavior of a rafted [001] oriented AM1 Ni-based si...
Single crystal Ni-based superalloy, with excellent mechanical properties in high temperature, always...