Relaxation times of bisphenol A polycarbonate around the glass transition temperature are estimated using the combination of differential scanning calorimetry (DSC) and thermostimulated depolarization currents (TSDC). These measurements are performed using samples with different thermal histories below and above the vitrification transformation. This protocol enables the extension of the range of equilibrium relaxation times measured by dielectric spectroscopy. By this mean we may recalculate the values of the Kauzmann temperature and fragility index
The isothermal cold-crystallization of the glass-former low-molecular-weight compound, ethylene glyc...
Resumen del trabajo presentado a la 10th Conference on Broadband Dielectric Spectroscopy and its App...
Starting from the Debye model for frequency dependent specific heat and the VFT model for its relaxa...
Relaxation times of bisphenol A polycarbonate around the glass transition temperature are estimated...
In this work, the variations of the relaxation times are investigated above and below the glass tran...
International audienceIn this work, the variations of the relaxation times are investigated above an...
In this paper we propose a new method of data analysis to interpret results obtained by Thermally S...
In this contribution, a dielectric measurement technique for the evaluation of phase transition temp...
The objective is to determine the glass transition temperature of a polymer using a dielectric dissi...
The vitrification of a glass-former can be driven by different physical-chemical processes: the usua...
Temperature-modulated differential scanning calorimetry (TMDSC) is based on conventional DSC but wit...
Annealed samples from a single melt of a 10 mol% K2O-90SiO2 glass were reheated to temperatures rang...
In the last decade the challenging analysis of previtreous behavior of relaxation time (Ï.,(T)) in u...
Starting from the Debye model for frequency-dependent specific heat and the Vogel-Fulcher-Tammann (V...
International audienceThe temperature dependence of characteristic length scales associated to the g...
The isothermal cold-crystallization of the glass-former low-molecular-weight compound, ethylene glyc...
Resumen del trabajo presentado a la 10th Conference on Broadband Dielectric Spectroscopy and its App...
Starting from the Debye model for frequency dependent specific heat and the VFT model for its relaxa...
Relaxation times of bisphenol A polycarbonate around the glass transition temperature are estimated...
In this work, the variations of the relaxation times are investigated above and below the glass tran...
International audienceIn this work, the variations of the relaxation times are investigated above an...
In this paper we propose a new method of data analysis to interpret results obtained by Thermally S...
In this contribution, a dielectric measurement technique for the evaluation of phase transition temp...
The objective is to determine the glass transition temperature of a polymer using a dielectric dissi...
The vitrification of a glass-former can be driven by different physical-chemical processes: the usua...
Temperature-modulated differential scanning calorimetry (TMDSC) is based on conventional DSC but wit...
Annealed samples from a single melt of a 10 mol% K2O-90SiO2 glass were reheated to temperatures rang...
In the last decade the challenging analysis of previtreous behavior of relaxation time (Ï.,(T)) in u...
Starting from the Debye model for frequency-dependent specific heat and the Vogel-Fulcher-Tammann (V...
International audienceThe temperature dependence of characteristic length scales associated to the g...
The isothermal cold-crystallization of the glass-former low-molecular-weight compound, ethylene glyc...
Resumen del trabajo presentado a la 10th Conference on Broadband Dielectric Spectroscopy and its App...
Starting from the Debye model for frequency dependent specific heat and the VFT model for its relaxa...