Abstract: This paper presents the results of an experimental investigation into the feasibility of deep-hole microdrilling a nickel-based superalloy. This material is very challenging to machine and current drilling methods are based on non-conventional machining technologies; the traditional view is that microdrills are too fragile to be used for drilling this high-strength aerospace alloy. The work investigated mechanical microdrilling under various cutting condi-tions. Mechanical microdrilling may offer the chance of improved hole quality and surface integrity. Initially a review of literature was undertaken with a view to identify the best drill geometry for the production of micro holes in nickel-based alloys. Based on this review the ...
International audienceInconel 718 Nickel-based superalloy has been applied widely in high temperatur...
The subject of this experiment was to produce parts with a specific shape and submillimetre elements...
The gas turbine, aerospace and nuclear industries are dependent upon nickel-based superalloys to ena...
Accomplishment of good dimensional accuracy and acceptable surface integrity in micro drilling of Ni...
Superalloys such as Inconel 718 have high strength at elevated temperatures, which make them attract...
Micro-drilling is an emerging substantial elimination process in the field of precision manufacturin...
AbstractWhite layers and extensive material drag introduced during rough machining are regarded as d...
AbstractNickel-based superalloys play a crucial role in elevated temperature applications where high...
In aerospace industry, the manufacturing of critical parts (high energy components) requires an impo...
The study focuses on the micro drilling of Incoloy 825 alloy under flood cutting condition. Micro dr...
Providing research equipment for the many and varied projects at Lawrence Livermore Laboratory leads...
This thesis was submitted for the award of Doctor of Philosophy and was awarded by Brunel University...
γ′-strengthened nickel-based superalloys are developed for high-performance systems such as jet engi...
© 2015 The Authors The main objective of this study is to investigate and optimize the hole roundnes...
AbstractThe main objective of this study is to investigate and optimize the hole roundness when dril...
International audienceInconel 718 Nickel-based superalloy has been applied widely in high temperatur...
The subject of this experiment was to produce parts with a specific shape and submillimetre elements...
The gas turbine, aerospace and nuclear industries are dependent upon nickel-based superalloys to ena...
Accomplishment of good dimensional accuracy and acceptable surface integrity in micro drilling of Ni...
Superalloys such as Inconel 718 have high strength at elevated temperatures, which make them attract...
Micro-drilling is an emerging substantial elimination process in the field of precision manufacturin...
AbstractWhite layers and extensive material drag introduced during rough machining are regarded as d...
AbstractNickel-based superalloys play a crucial role in elevated temperature applications where high...
In aerospace industry, the manufacturing of critical parts (high energy components) requires an impo...
The study focuses on the micro drilling of Incoloy 825 alloy under flood cutting condition. Micro dr...
Providing research equipment for the many and varied projects at Lawrence Livermore Laboratory leads...
This thesis was submitted for the award of Doctor of Philosophy and was awarded by Brunel University...
γ′-strengthened nickel-based superalloys are developed for high-performance systems such as jet engi...
© 2015 The Authors The main objective of this study is to investigate and optimize the hole roundnes...
AbstractThe main objective of this study is to investigate and optimize the hole roundness when dril...
International audienceInconel 718 Nickel-based superalloy has been applied widely in high temperatur...
The subject of this experiment was to produce parts with a specific shape and submillimetre elements...
The gas turbine, aerospace and nuclear industries are dependent upon nickel-based superalloys to ena...