In the present work is determined, the increase in erosive wear resistance to cavitation, TiN coatings obtained by physical vapour deposition (PVD) on aluminium (99 % commercially pure). The wear tests were performed by vibratory cavitation in bioethanol-gasoline mixtures with concentrations of 5 % to 30%, in order to study the evolution of erosive wear by cavitation. The characterization after deterioration test was performed by scanning electron microscopy for the different testing times. Because of the cavitation test, the mass loss was determined and, sequential study of the surface appearance of the samples was done to determine the wear mechanisms prevailing in each stage. The results were analysed by atomic force microscopy character...
The evolution of surface roughness of three common metallic materials (316L stainless steel, CP tita...
Cavitation erosion tests were carried out by using vibratory apparatus to obtain MDE (Mean Depth of ...
The resistance to cavitation erosion and sliding wear of stainless steel grade AISI 304 can be impro...
This article presents the evaluation of the corrosion erosion resistance erosion caused by cavitatio...
Cavitation erosion is a phenomenon that occurs when the pressure of the liquid drops below its vapou...
In this work is presented the results of the corrosion erosion resistance evaluation by cavitation o...
This manuscript deals with the cavitation erosion resistance of flame-sprayed Al2O3-40%TiO2/NiMoAl c...
Cavitation erosion tests were carried out on 10 kinds of base metals such as irons and stainless ste...
Cavitation erosion-corrosion of nickel aluminium bronze with oxide films formed under two different ...
The relevance of the research is caused by the need to study the resistance of metals and their coat...
Two kinds of Ti-alloys, i.e., Al–5Ti and Al–10Ti alloys, were manufactured in this study, and their ...
Following a preceding report, this paper summarises preliminary results for the study of PVD TiN coa...
Within a research project regarding cavitation erosion-resistant coatings, arc spraying was used wit...
Research on Nano layer coating application for the improvement of the resistance to cavitation erosi...
This article presents the results of the research related to the experimental behavior of alumina co...
The evolution of surface roughness of three common metallic materials (316L stainless steel, CP tita...
Cavitation erosion tests were carried out by using vibratory apparatus to obtain MDE (Mean Depth of ...
The resistance to cavitation erosion and sliding wear of stainless steel grade AISI 304 can be impro...
This article presents the evaluation of the corrosion erosion resistance erosion caused by cavitatio...
Cavitation erosion is a phenomenon that occurs when the pressure of the liquid drops below its vapou...
In this work is presented the results of the corrosion erosion resistance evaluation by cavitation o...
This manuscript deals with the cavitation erosion resistance of flame-sprayed Al2O3-40%TiO2/NiMoAl c...
Cavitation erosion tests were carried out on 10 kinds of base metals such as irons and stainless ste...
Cavitation erosion-corrosion of nickel aluminium bronze with oxide films formed under two different ...
The relevance of the research is caused by the need to study the resistance of metals and their coat...
Two kinds of Ti-alloys, i.e., Al–5Ti and Al–10Ti alloys, were manufactured in this study, and their ...
Following a preceding report, this paper summarises preliminary results for the study of PVD TiN coa...
Within a research project regarding cavitation erosion-resistant coatings, arc spraying was used wit...
Research on Nano layer coating application for the improvement of the resistance to cavitation erosi...
This article presents the results of the research related to the experimental behavior of alumina co...
The evolution of surface roughness of three common metallic materials (316L stainless steel, CP tita...
Cavitation erosion tests were carried out by using vibratory apparatus to obtain MDE (Mean Depth of ...
The resistance to cavitation erosion and sliding wear of stainless steel grade AISI 304 can be impro...